Acta Metallurgica Sinica (English Letters) ›› 2017, Vol. 30 ›› Issue (1): 66-72.DOI: 10.1007/s40195-016-0509-8
Special Issue: 2017-2018镁合金专辑
• Orginal Article • Previous Articles Next Articles
Zhan-Yong Zhao1(
),Ren-Guo Guan2(
),Jian-Hong Zhang1,Zhou-Yang Zhao2,Pei-Kang Bai1
Received:2016-07-28
Online:2017-02-16
Published:2017-02-16
Zhan-Yong Zhao,Ren-Guo Guan,Jian-Hong Zhang,Zhou-Yang Zhao,Pei-Kang Bai. Effects of Process Parameters of Semisolid Stirring on Microstructure of Mg-3Sn-1Mn-3SiC (wt%) Strip Processed by Rheo-rolling[J]. Acta Metallurgica Sinica (English Letters), 2017, 30(1): 66-72.
Fig. 2 SEM image a and EDS b from the position Aa of Mg-3Sn-1Mn-3SiC (wt%) composite obtained at stirring temperatures 680 °C (stirring speeds 800 rpm, stirring time 15 min)
Fig. 3 Microstructures of Mg-3Sn-1Mn-3SiC (wt%) composites prepared under different stirring temperatures (stirring speeds 800 rpm, stirring time 15 min): a 680 °C, b 660 °C, c 640 °C
Fig. 5 SEM image and EDS of Mg-3Sn-1Mn-3SiC (wt%) composites under different stirring speeds (stirring time was 15 min, and stirring temperature was 640 °C): a 500 rpm; c 1100 rpm, EDS, b from point Ba EDS, d from point Cc
Fig. 6 Microstructures of Mg-3Sn-1Mn-3SiC (wt%) composites under different stirring speeds (stirring time was 15 min, and stirring temperature was 640 °C): a 500 rpm; b 1100 rpm
Fig. 7 Relationships among the stirring speed and α-Mg grain diameter as well as roundness (stirring time was 15 min, and stirring temperature was 640 °C)
Fig. 8 Microstructures of Mg-3Sn-1Mn-3SiC (wt%) composites under different stirring time (stirring speed at 1100 rpm, stirring temperature at 640 °C): a 5 min, b 30 min
|
| [1] | Shang Zhao, Zhaolin Wang, Mingliang Wang, Zeyu Ding, Yiping Lu. A critical review of advances and application prospects of soft magnetic high entropy alloys [J]. Metals Advances, 2026, 40(2): 1-7. |
| [2] | Wei-Peng Chen, Jia-Qi Pei, Hua Hou, Yu-Hong Zhao. Phase-field simulation of α-Mg dendrite growth in magnesium alloys: A review [J]. Metals Advances, 2026, 40(2): 48-61. |
| [3] | Peng Han, Wen Wang, Jun Cai, Jia Lin, Hubin Yang, Qianzhi Ma, Feng Gao, Ke Qiao, Fengming Qiang, Kuaishe Wang. Excellent superplasticity for lamellar microstructure in nugget of a double-sided friction stir welded Ti-4.5Al-3V-2Mo-2Fe alloy joint [J]. Metals Advances, 2026, 40(2): 110-123. |
| [4] | Lei Qin, Shengfeng Zhou, Jianbo Jin, Huan Yang, Kunmao Li, Cheng Deng, Yujie Yuan, Seyed Reza Elmi Hosseini, Lai-Chang Zhang. Effect of molybdenum content on the microstructure and tribological properties of Ti-Nb-Cu alloys produced by LPBF additive manufacturing [J]. Metals Advances, 2026, 39(1): 13-25. |
| [5] | X.L. Wang, J.Y. Li, Q.S. Mei. Recent progress in Zn matrix composites for biomedical applications [J]. Metals Advances, 2026, 39(1): 26-37. |
| [6] | Kunmao Li, Shengfeng Zhou, Jing Liu, Feng Yang, Chengliang Yang. A review on the biomedical Ti-Cu alloys: Design, preparation, microstructure and properties [J]. Metals Advances, 2026, 39(1): 47-67. |
| [7] | Huihui Wang, Qianying Guo, Chong Li, Lei Cui, Yiming Huang, Yongchang Liu. Effect of Ti2AlC Addition on the Microstructure and Mechanical Property of Additive Manufactured Inconel 718 Alloys via Laser Powder Bed Fusion [J]. Acta Metallurgica Sinica (English Letters), 2025, 38(9): 1481-1498. |
| [8] | B. M. Shi, Y. T. Pang, B. H. Shan, B. B. Wang, Y. Liu, P. Xue, J. F. Zhang, Y. N. Zan, Q. Z. Wang, B. L. Xiao, Z. Y. Ma. Microstructure Evolution and Fracture Behavior of (B4C+Al2O3)/Al Friction Stir Welded Joints [J]. Acta Metallurgica Sinica (English Letters), 2025, 38(9): 1513-1526. |
| [9] | H. Q. Dai, N. Li, L. H. Wu, J. Wang, P. Xue, F. C. Liu, D. R. Ni, B. L. Xiao, Z. Y. Ma. Low-Temperature Superplastic Deformation Behavior of Bimodal Microstructure of Friction Stir Processed Ti-6Al-4V Alloy [J]. Acta Metallurgica Sinica (English Letters), 2025, 38(9): 1559-1569. |
| [10] | Shuyi Ren, Jiao Li, Kai Wu, Xiaoge Li, Yaqiang Wang, Jinyu Zhang, Gang Liu, Jun Sun. Thermal Stability and Mechanical Properties of Nanotwinned Ni-W Alloyed Films [J]. Acta Metallurgica Sinica (English Letters), 2025, 38(9): 1570-1582. |
| [11] | F. S. Li, L. H. Wu, Y. Kan, H. B. Zhao, D. R. Ni, P. Xue, B. L. Xiao, Z. Y. Ma. Microstructure Evolution and Fracture Mechanisms in Electron Beam Welded Joint of Ti-6Al-4V ELI Alloy Ultra-thick Plates [J]. Acta Metallurgica Sinica (English Letters), 2025, 38(8): 1317-1330. |
| [12] | Haoran Pang, Liwei Lu, Gongji Yang, Xiaojun Wang, Wen Wang, Hua Zhang, Yujuan Wu. Amelioration of Mechanical Properties of Rolled Mg-4.5Al-2.5Zn Alloy by Cryogenic Cycling Treatment [J]. Acta Metallurgica Sinica (English Letters), 2025, 38(8): 1436-1452. |
| [13] | Yunlu Jiang, Lihui Wu, Dingrui Ni, Hongbo Zhao, Xu Han, Peng Xue, Bolv Xiao, Zongyi Ma. Effect of Post Weld Heat Treatment on Residual Stress and Mechanical Properties of 106 mm Thick TC4 Titanium Alloy Electron Beam Welded Joints [J]. Acta Metallurgica Sinica (English Letters), 2025, 38(7): 1083-1094. |
| [14] | Qi Zhou, Yufeng Xia, Yu Duan, Baihao Zhang, Yuqiu Ye, Peitao Guo, Lu Li. Microstructure and Mechanical Properties of Yb-Containing AZ80 Cast Alloys [J]. Acta Metallurgica Sinica (English Letters), 2025, 38(7): 1095-1108. |
| [15] | Tiantian Wang, Lin Liu, Zexin Liu, Kang Wang, Runhua Yao, Xiaohong Yao, Ruiqiang Hang. Characterization, Mechanical Property, Degradation Behavior, and Osteogenic Activity of Zn-Mn Alloy Foam Prepared by Electrodeposition [J]. Acta Metallurgica Sinica (English Letters), 2025, 38(7): 1157-1173. |
| Viewed | ||||||
|
Full text |
|
|||||
|
Abstract |
|
|||||
WeChat