Abstract

The influence of temperature on the hydrogen diffusion behavior in X80 pipeline steel during stacking for slow cooling was studied using electrochemical penetration method, the temperature field and the hydrogen diffusion in this pipeline steel during stacking for slow cooling were simulated by ABAQUS finite element method (FEM) software. The results show that in this process there is a reciprocal relationship between the natural logarithm of hydrogen diffusion coefficient and temperature. The cooling rate decreases gradually with the increase of steel plate thickness. The hydrogen content is higher at high temperature (500–400 °C) than that in low temperature region (300–100 °C). The FEM simulation results are consistent with the experimental ones, and the model can be used to predict the hydrogen diffusion behavior in industrial production of X80 pipeline steel.

Cite this article

Zhenyi Huang , Qi Shi , Fuqiang Chen , Yunfeng Shi . FEM Simulation of the Hydrogen Diffusion in X80 Pipeline Steel During Stacking for Slow Cooling[J]. Acta Metallurgica Sinica (English Letters), 2014 , 27(3) : 416 -421 . DOI: 10.1007/s40195-014-0073-z

References

[1] H. Kin, B.N. Popov, K.S. Chen, Corros. Sci. 45, 1005(2003)
[2] A. Caravella, N. Hara, H. Negishi, S. Hara, Hydrog. Energy 39, 4676(2014)10.1016/j.ijhydene.2013.10.015
[3] I. Moro, L. Briottet, P. Lemoine, E. Andrieu, C. Blanc, Mater. Sci. Eng. A 527, 7252(2010)10.1016/j.msea.2010.07.027
[4] C.Y. Yan, C.Y. Liu, B. Yan, Comput. Mater. Sci. 83, 158(2014)10.1016/j.commatsci.2013.11.007
[5] T. Zhang, Y. Yao, W.Y. Chu, L.J. Qiao, Acta Metall. Sin. 38, 844(2002). (in Chinese)
[6] M. Mukherjee, T.K. Pal, Acta Metall. Sin. (Engl. Lett.) 26, 206(2013)10.1007/s40195-012-0200-7
[7] F.L. Sun, X.G. Li, F. Zhang, X.Q. Cheng, C. Zhou, N.C. Wu, Y.Q. Yin, J.B. Zhao, Acta Metall. Sin. (Engl. Lett.) 26, 257(2013)10.1007/s40195-012-0231-0
[8] C.L. Qiu, L.Y. Lan, D.W. Zhao, X.H. Gao, L.X. Du, Acta Metall. Sin. (Engl. Lett.) 26, 49(2013)10.1007/s40195-012-0103-7
[9] Z.T. Liu, C.W. Du, X. Zhang, F.M. Wang, X.G. Li, Acta Metall. Sin. (Engl. Lett.) 26, 489(2013)10.1007/s40195-012-0216-z
[10] Y.X. Wu, D. Tang, H.T. Jiang, Z.L. Mi, H.T. Jing, Acta Metall. Sin. (Engl. Lett.) 26, 713(2013)10.1007/s40195-013-0232-7
[11] H.Y. Song, S.H. Zhang, L.Y. Lan, C.M. Li, H.T. Liu, D.W. Zhao, G.D. Wang, Acta Metall. Sin. (Engl. Lett.) 26, 390(2013)10.1007/s40195-012-0183-4
[12] M.A.V. Devanathan, Z. Stachushi, Proc. R. Soc. 270, 90(1962)10.1098/rspa.1962.0205
[13] H.B. Xue, Y.F. Cheng, Corros. Sci. 53, 1201(2011)10.1016/j.corsci.2010.12.011
[14] Y.X. Chen, Q.G. Chang, Acta Metall. Sin. 47, 548(2011). (in Chinese)
[15] D. Oaoh, G. Owolabi, A. Odeshi, H. Whitworth, Acta Metall. Sin. (Engl. Lett.) 26, 378(2013)10.1007/s40195-013-0103-2
[16] R.A. Oriani, Acta Metall. 18, 147(1970)10.1016/0001-6160(70)90078-7
[17] Y.D. Han, Mater. Chem. Phys. 132, 216(2012)10.1016/j.matchemphys.2011.11.036
[18] S. Liu, H. Zheng, Q.H. Gui, A.H. Ma, H.B. Yu, L.B. Wang, H.G. Yang, Acta Metall. Sin. 40, 393(2004). (in Chinese)
[19] K. Masui, H. Yoshida, R. Watanabe, Trans. ISIJ 19, 547(1979)
[20] T. Tanabe, Y. Yamanishi, S. Imoto, Mater. Trans. JIM 25, 1(1984)
[21] J. Xu, X.K. Sun, W.X. Chen, Y.Y. Li, Acta Metall. Sin. 28, 399(1992). (in Chinese)
Options
Outlines

/