Research paper

Forming process and numerical simulation of making upset on oil drill pipe

  • HAO Zhang-Qian
Expand
  • 1. School of Mechanical and Electrical Engineering, Central South University, Changsha 410083, China
    2. School of Mechanical Engineering, Nantong University, Nantong 226007, China

Received date: 2009-08-12

  Revised date: 2009-12-06

  Online published: 2010-02-09

Abstract

The flow stress behavior of grade G-105 steel (API  standard) for oil drill pipe in hot compressive deformation was  studied by isothermal compression tests on Gleeble-1500  thermal-mechanical machine. Referring to established empirical  formulas, the constitutive equation of the flow stress for G-105  steel was obtained. For the grade G-105 oil drill pipe  (φ114.3×10.92 mm), through proper design of the die and  applying suitable process parameters, and using coupled rigid  viscoplastic thermo-mechanical finite element method, the forming  process of making upset on oil drill pipe was numerically simulated.  The simulation results show that the internal transition section of  the oil drill pipe is not only continuous and smooth but also long  (up to about 220-250mm).

Cite this article

HAO Zhang-Qian . Forming process and numerical simulation of making upset on oil drill pipe[J]. Acta Metallurgica Sinica (English Letters), 2010 , 23(1) : 72 -80 . DOI: 10.11890/1006-7191-101-72

References

[1] B.M. Wang,  The Process of Oil Drill Pipe in Foreign  (Metallurgical Industry Press, Beijing, 1983) p.3 (in Chinese).
[2] API SPECIFICATION 5D. Specification for Drill Pipe [S]p.12.
[3] W.G. Chunn and W. R.T. Moore,  US US5184495  (9 February 1993).
[4] T.E. Winship,  US US5517843  (21 May 1996).
[5] E. Takeuchi and H. Miyoshi,  US US4845972  (11 July 1989).
[6] S.S. Xie and L. Li,  Finite Element Simulation Technology and Its Application in Metal Forming  (Science press, Beijing, 2008) p.1 (in Chinese).
[7] H.G. Zhang, Y. He, X.F. Liu and J.X. Xie,  Acta Metall Sin  43  (2007) 930 (in Chinese).
[8] J.M. Zhou, L.H. Qi and G.D. Chen,  Mech Sci Technol  14  (2005) 212 (in Chinese).
[9] S.L. Wang, X.Y. Ruan and X.L. Yu,  J Shanghai Jiaotong Univ  30  (1996) 20 (in Chinese).
[10] Y.S. Xu, J.T. Liu and M. Nie,  J Appl Sci  15 (1997) 379 (in Chinese).
[11] P. Zhao and J.W. Zhang,  CN CN200510027402  (3 January 2007).
[12] J.W. Zhang and W. Wang,  CN CN200610028551  (2 January 2008).
[13] Z.Z. Chen and D.N. Lan,  Die Steel Manual  (Metallurgical Industry Press, Beijing, 2002) p.370 (in Chinese).
[14] H.X. Li,  Friction and Lubrication in Pressure Processing  (Metallurgical Industry Press, Beijing, 1993) p.132(in Chinese).
[15] D.N. Wang,  Principal of Metal Plastic Forming (China Machine Press, Beijing, 1982) p.109 (in Chinese).

Outlines

/